DILLINAL 460/630 (EN P460M)
DILLINAL 460/630 (EN P460M) introduction
DILLINAL 460/630 is a weldable normalized fine grained steel which is characterised by a minimum yield
strength of 460 MPa and a minimum tensile strength of 630 MPa.
DILLINAL 460/630 is mainly applied for the construction of tanks for the transport of liquefied gas with road
and rail vehicles where the weight minimisation plays an important role.
DIILINAL 460/630 can be supplied in two qualities: DILLINAL 460/630 N and DILLINAL 460/630 NL. They
are both modified steels of the type P460 according to EN 10028-3. They fulfill the requirements of
EN 10028-3:2009 (option 5 and footnote d, Table 4) and the VdTÜV- material data sheet 531 "Hochfester,
legierter Feinkornbaustahl460/630 für Einsatztemperaturen bis -40 °C" (High Strength Alloyed Fine Grained
Steel 460/630 for service temperatures down to -40 °C)
This material data sheet applies to heavy plates with thicknesses from 7 to 20 mm.
DILLINAL 460/630 (EN P460M) general
Property |
Temperature |
Value |
Comment |
Charpy impact energy, V-notch |
-40 °C |
Charpy impact energy, V-notch of 27 J |
option 1 | Dillinal 460/630 NL | average of 3 tests | transverse specimens | *The specified values are minimum values for the average of 3 tests. No individual value is to be less than 70 % of the specified minimum. For plate thickness below 11 mm the test can be carried out on Charpy-V specimens or Charpy-V-type specimens with reduced width. The minimum impact value will be reduced proportionally to the reduction of the specimen’s cross section |
- |
-40 °C |
Charpy impact energy, V-notch of 45 J |
option 2 (to be indicated on the order) | Dillinal 460/630 NL | average of 3 tests | transverse specimens | * |
- |
-20 °C |
Charpy impact energy, V-notch of 27 J |
option 1 | Dillinal 460/630 N | average of 3 tests | transverse specimens | * |
- |
-20 °C |
Charpy impact energy, V-notch of 45 J |
option 2 (to be indicated on the order) | Dillinal 460/630 N | average of 3 tests | transverse specimens | * |
Elongation |
- |
Elongation of 17 % |
min. for plate thickenss t ≤ 20 mm | transverse specimens, A5 |
Tensile strength |
- |
Tensile strength of 630 - 725 MPa |
for plate thickness t ≤ 20 mm | transverse specimens |
Yield strength |
- |
Yield strength of 460 MPa |
min. ReH for plate thickness t ≤ 20 mm | transverse specimens |
DILLINAL 460/630 (EN P460M) chemical
Property |
Value |
Comment |
Carbon |
Carbon of 0.2 % |
max. heat |
- |
Carbon of 0.22 % |
max. product |
Chromium |
Chromium of 0.3 % |
max. heat |
- |
Chromium of 0.35 % |
max. product |
Copper |
Copper of 0.2 % |
max. heat |
- |
Copper of 0.25 % |
max. product |
Iron |
- |
Manganese |
Manganese of 0.94 - 1.8 % |
product |
- |
Manganese of 1 - 1.7 % |
heat |
Molybdenum |
Molybdenum of 0.1 % |
max. heat |
- |
Molybdenum of 0.13 % |
max. product |
Nickel |
Nickel of 0.4 % |
max. heat |
- |
Nickel of 0.45 % |
max. product |
Nitrogen |
Nitrogen of 0.025 % |
max. heat |
- |
Nitrogen of 0.027 % |
max. product |
Other |
Other of 0.45 % |
max. Cu+Cr+Mo for heat only |
Phosphorus |
Phosphorus of 0.02 % |
max. heat |
- |
Phosphorus of 0.025 % |
max. product |
Silicon |
Silicon of 0.1 - 0.6 % |
heat |
- |
Silicon of 0.1 - 0.65 % |
product |
Sulfur |
Sulfur of 0.005 % |
max. heat |
- |
Sulfur of 0.008 % |
max. product |
Vanadium |
Vanadium of 0.1 - 0.21 % |
product |
- |
Vanadium of 0.1 - 0.2 % |
heat |