BS 970-1 Grade 605M36
Equivalent material: BS EN16
BS 970-1 Grade 605M36 general
| Property | Temperature | Value |
|---|---|---|
| Elongation | 20.0 °C | Elongation of 15 - 17 % |
| Hardness, Brinell | 20.0 °C | Hardness, Brinell of 201 - 255 [-] |
| Tensile strength | 20.0 °C | Tensile strength of 700 - 850 MPa |
| Yield strength | 20.0 °C | Yield strength of 495 - 525 MPa |
| Yield strength Rp0.2 | 20.0 °C | Yield strength Rp0.2 of 480 - 510 MPa |
BS 970-1 Grade 605M36 chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.32 - 0.4 % |
| Iron | Balance |
| Manganese | Manganese of 1.3 - 1.7 % |
| Molybdenum | Molybdenum of 0.22 - 0.32 % |
| Phosphorus | Phosphorus of 0.04 % |
| Silicon | Silicon of 0.1 - 0.4 % |
| Sulfur | Sulfur of 0.04 % |