ASTM Alloy 1 Cold-Rolled Hard Temper
Equivalent material: UNS K94490
ASTM Alloy 1 Cold-Rolled Hard Temper general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 8.8 g/cm³ |
Typical for Nickel Steel |
ASTM Alloy 1 Cold-Rolled Hard Temper thermal
| Property |
Temperature |
Value |
Comment |
| Melting point |
- |
Melting point of 1316 - 1595 °C |
Typical for Nickel Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 456 J/(kg·K) |
Typical for Nickel Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 10 - 50 W/(m·K) |
Typical for Nickel Steel |
ASTM Alloy 1 Cold-Rolled Hard Temper chemical
| Property |
Value |
| Carbon |
Carbon of 0.05 % |
| Chromium |
Chromium of 0.3 % |
| Cobalt |
Cobalt of 0.5 % |
| Copper |
Copper of 0.3 % |
| Manganese |
Manganese of 0.8 % |
| Molybdenum |
Molybdenum of 0.3 % |
| Nickel |
Nickel of 43.5 - 46.5 % |
| Phosphorus |
Phosphorus of 0.03 % |
| Silicon |
Silicon of 0.5 % |
| Sulfur |
Sulfur of 0.01 % |
ASTM Alloy 1 Cold-Rolled Hard Temper mechanical
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Steel |
| Elongation A50 |
23.0 °C |
Elongation A50 of 2 % |
- |
| Hardness, Rockwell Superficial 15-N |
23.0 °C |
Hardness, Rockwell Superficial 15-N of 74 [-] |
- |
| Hardness, Vickers |
23.0 °C |
Hardness, Vickers of 270 [-] |
- |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Steel |
| Shear modulus |
23.0 °C |
Shear modulus of 76 GPa |
Typical for Nickel Steel |
| Tensile strength |
23.0 °C |
Tensile strength of 827 MPa |
- |
| Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 793 MPa |
- |