ASTM A982 Grade A Class 2 Quenched and Tempered; Stress-Relieved
ASTM A982 Grade A Class 2 Quenched and Tempered; Stress-Relieved general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
ASTM A982 Grade A Class 2 Quenched and Tempered; Stress-Relieved thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Melting point | - | Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
ASTM A982 Grade A Class 2 Quenched and Tempered; Stress-Relieved mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | Charpy impact energy of 33 J | - |
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 | 23.0 °C | Elongation A50 of 18 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 269 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Reduction of area | 23.0 °C | Reduction of area of 50 % | - |
Tensile strength | 23.0 °C | Tensile strength of 760 MPa | - |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 555 MPa | - |
Let our high-quality steel be the cornerstone of your architectural masterpieces and engineering marvels.
-- Our promise
Get a quote