ASTM A958 Grade SC4330 Class 65/35, Heat-Treated
Equivalent material: ASTM Grade SC4330, UNS J23259
ASTM A958 Grade SC4330 Class 65/35, Heat-Treated general
Property |
Temperature |
Value |
Comment |
Density |
20.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A958 Grade SC4330 Class 65/35, Heat-Treated thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
20.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Nickel Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 34 - 54 W/(m·K) |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A958 Grade SC4330 Class 65/35, Heat-Treated chemical
Property |
Value |
Carbon |
Carbon of 0.28 - 0.33 % |
Chromium |
Chromium of 0.7 - 0.9 % |
Manganese |
Manganese of 0.6 - 0.9 % |
Molybdenum |
Molybdenum of 0.2 - 0.3 % |
Nickel |
Nickel of 1.65 - 2 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.3 - 0.6 % |
Sulfur |
Sulfur of 0.04 % |
ASTM A958 Grade SC4330 Class 65/35, Heat-Treated mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 |
20.0 °C |
Elongation A50 of 24 % |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Chromium Molybdenum Steel |
Reduction of area |
20.0 °C |
Reduction of area of 35 % |
- |
Tensile strength |
20.0 °C |
Tensile strength of 450 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 240 MPa |
- |