ASTM A920 Grade 15V41 Class 520, Hot-Wrought
Equivalent material: ASTM Grade 15V41
ASTM A920 Grade 15V41 Class 520, Hot-Wrought general
Property |
Temperature |
Value |
Comment |
Density |
20.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Molybdenum Steel |
ASTM A920 Grade 15V41 Class 520, Hot-Wrought thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
20.0 °C |
Coefficient of thermal expansion of 1.29E-5 1/K |
Typical for Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Molybdenum Steel |
Specific heat capacity |
20.0 °C |
Specific heat capacity of 456 J/(kg·K) |
Typical for Molybdenum Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 37 - 48 W/(m·K) |
Typical for Molybdenum Steel |
ASTM A920 Grade 15V41 Class 520, Hot-Wrought chemical
Property |
Value |
Carbon |
Carbon of 0.36 - 0.44 % |
Manganese |
Manganese of 1.35 - 1.65 % |
Molybdenum |
Molybdenum of 0.01 - 0.3 % |
Niobium |
Niobium of 0.01 - 0.07 % |
Phosphorus |
Phosphorus of 0.04 % |
Sulfur |
Sulfur of 0.05 % |
Vanadium |
Vanadium of 0.02 - 0.2 % |
ASTM A920 Grade 15V41 Class 520, Hot-Wrought mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Molybdenum Steel |
Elongation A200 |
20.0 °C |
Elongation A200 of 7 % |
- |
Elongation A50 |
20.0 °C |
Elongation A50 of 10 % |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Molybdenum Steel |
Tensile strength |
20.0 °C |
Tensile strength of 690 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 520 MPa |
- |
Collaborate with us to explore innovative possibilities using our cutting-edge steel technologies.
-- Our promise
Similar or equivalent steel materials
Get a quote