ASTM A860 Grade WPHY 65 Heat-Treated
ASTM A860 Grade WPHY 65 Heat-Treated general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
ASTM A860 Grade WPHY 65 Heat-Treated thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.33E-5 1/K | Typical for Manganese Steel |
Melting point | - | Melting point of 1382 - 1529 °C | Typical for Manganese Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 14 - 16 W/(m·K) | Typical for Manganese Steel |
ASTM A860 Grade WPHY 65 Heat-Treated chemical
Property | Value |
---|---|
Aluminium | Aluminium of 0.06 % |
Carbon | Carbon of 0.2 % |
Chromium | Chromium of 0.3 % |
Copper | Copper of 0.35 % |
Manganese | Manganese of 1 - 1.45 % |
Molybdenum | Molybdenum of 0.25 % |
Nickel | Nickel of 0.5 % |
Niobium | Niobium of 0.04 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.15 - 0.4 % |
Sulfur | Sulfur of 0.01 % |
Titanium | Titanium of 0.05 % |
Vanadium | Vanadium of 0.1 % |
ASTM A860 Grade WPHY 65 Heat-Treated mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | Charpy impact energy of 40 J | - |
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Manganese Steel |
Elongation A50 | 23.0 °C | Elongation A50 of 28 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 235 [-] | - |
Hardness, Rockwell C | 23.0 °C | Hardness, Rockwell C of 22 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Manganese Steel |
Tensile strength | 23.0 °C | Tensile strength of 530 - 705 MPa | - |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 450 MPa | - |
Benefit from our expertise in precision engineering to achieve superior steel solutions.
-- Our promise
Get a quote