ASTM A860 Grade WPHY 46 Heat-Treated

ASTM A860 Grade WPHY 46 Heat-Treated general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Manganese Steel

ASTM A860 Grade WPHY 46 Heat-Treated thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.33E-5 1/K Typical for Manganese Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Manganese Steel
Specific heat capacity 23.0 °C Specific heat capacity of 510 - 553 J/(kg·K) Typical for Manganese Steel
Thermal conductivity 23.0 °C Thermal conductivity of 14 - 16 W/(m·K) Typical for Manganese Steel

ASTM A860 Grade WPHY 46 Heat-Treated chemical

Property Value
Aluminium Aluminium of 0.06 %
Carbon Carbon of 0.2 %
Chromium Chromium of 0.3 %
Copper Copper of 0.35 %
Manganese Manganese of 1 - 1.45 %
Molybdenum Molybdenum of 0.25 %
Nickel Nickel of 0.5 %
Niobium Niobium of 0.04 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.15 - 0.4 %
Sulfur Sulfur of 0.01 %
Titanium Titanium of 0.05 %
Vanadium Vanadium of 0.1 %

ASTM A860 Grade WPHY 46 Heat-Treated mechanical

Property Temperature Value Comment
Charpy impact energy 23.0 °C Charpy impact energy of 40 J -
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Manganese Steel
Elongation A50 23.0 °C Elongation A50 of 32 % -
Hardness, Brinell 23.0 °C Hardness, Brinell of 235 [-] -
Hardness, Rockwell C 23.0 °C Hardness, Rockwell C of 22 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Manganese Steel
Tensile strength 23.0 °C Tensile strength of 435 - 605 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 315 MPa -