ASTM A757 Grade B4N Normalized and Tempered
Equivalent material: ASTM B4N, ASTM Grade B4Q, ASTM B4Q, UNS J41501
ASTM A757 Grade B4N Normalized and Tempered general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 8.8 g/cm³ |
Typical for Nickel Steel |
ASTM A757 Grade B4N Normalized and Tempered thermal
Property |
Temperature |
Value |
Comment |
Melting point |
- |
Melting point of 1316 - 1595 °C |
Typical for Nickel Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 456 J/(kg·K) |
Typical for Nickel Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 10 - 50 W/(m·K) |
Typical for Nickel Steel |
ASTM A757 Grade B4N Normalized and Tempered chemical
Property |
Value |
Carbon |
Carbon of 0.15 % |
Manganese |
Manganese of 0.5 - 0.8 % |
Nickel |
Nickel of 4 - 5 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.6 % |
Sulfur |
Sulfur of 0.025 % |
ASTM A757 Grade B4N Normalized and Tempered mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
23.0 °C |
Charpy impact energy of 20 J |
- |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 24 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Steel |
Reduction of area |
23.0 °C |
Reduction of area of 35 % |
- |
Shear modulus |
23.0 °C |
Shear modulus of 76 GPa |
Typical for Nickel Steel |
Tensile strength |
23.0 °C |
Tensile strength of 485 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 275 MPa |
- |