ASTM A752 Grade 5147 Annealed

Equivalent material: UNS G51470

ASTM A752 Grade 5147 Annealed general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Chromium Steel

ASTM A752 Grade 5147 Annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K Typical for Chromium Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Chromium Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 - 494 J/(kg·K) Typical for Chromium Steel
Thermal conductivity 23.0 °C Thermal conductivity of 23 - 50 W/(m·K) Typical for Chromium Steel

ASTM A752 Grade 5147 Annealed chemical

Property Value
Carbon Carbon of 0.46 - 0.51 %
Chromium Chromium of 0.85 - 1.15 %
Copper Copper of 0.35 %
Manganese Manganese of 0.7 - 0.95 %
Molybdenum Molybdenum of 0.06 %
Nickel Nickel of 0.25 %
Phosphorus Phosphorus of 0.04 %
Silicon Silicon of 0.15 - 0.35 %
Sulfur Sulfur of 0.04 %

ASTM A752 Grade 5147 Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Chromium Steel
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Chromium Steel
Tensile strength 23.0 °C Tensile strength of 680 MPa -