ASTM A732 Grade 6N Normalized and Tempered
Equivalent material: ASTM IC 4020
ASTM A732 Grade 6N Normalized and Tempered general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
ASTM A732 Grade 6N Normalized and Tempered thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.33E-5 1/K | Typical for Manganese Steel |
| Melting point | - | Melting point of 1382 - 1529 °C | Typical for Manganese Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 14 - 16 W/(m·K) | Typical for Manganese Steel |
ASTM A732 Grade 6N Normalized and Tempered chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.35 % |
| Manganese | Manganese of 1.35 - 1.75 % |
| Molybdenum | Molybdenum of 0.25 - 0.55 % |
| Phosphorus | Phosphorus of 0.04 % |
| Silicon | Silicon of 0.2 - 0.8 % |
| Sulfur | Sulfur of 0.045 % |
ASTM A732 Grade 6N Normalized and Tempered mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Manganese Steel |
| Elongation A50 | 23.0 °C | Elongation A50 of 20 % | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Manganese Steel |
| Tensile strength | 23.0 °C | Tensile strength of 621 MPa | - |
| Yield strength | 23.0 °C | Yield strength of 414 MPa | - |
Embrace sustainable practices with our eco-friendly steel solutions for a greener future.
-- Our promise

Get a quote