ASTM A681 Grade Type A7 Cold Drawn

Equivalent material: UNS T30107

ASTM A681 Grade Type A7 Cold Drawn general

Property Temperature Value Comment
Density 23.0 °C Density of 7.72 - 8 g/cm³ Typical for Tool And Machining Steel

ASTM A681 Grade Type A7 Cold Drawn thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K Typical for Tool And Machining Steel
Melting point - Melting point of 1370 - 1425 °C Typical for Tool And Machining Steel
Specific heat capacity 23.0 °C Specific heat capacity of 420 - 460 J/(kg·K) Typical for Tool And Machining Steel
Thermal conductivity 23.0 °C Thermal conductivity of 17 - 42 W/(m·K) Typical for Tool And Machining Steel

ASTM A681 Grade Type A7 Cold Drawn chemical

Property Value
Carbon Carbon of 2 - 2.85 %
Chromium Chromium of 5 - 5.75 %
Manganese Manganese of 0.2 - 0.8 %
Molybdenum Molybdenum of 0.9 - 1.4 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.1 - 0.7 %
Sulfur Sulfur of 0.03 %
Tungsten Tungsten of 0.5 - 1.5 %
Vanadium Vanadium of 3.9 - 5.15 %

ASTM A681 Grade Type A7 Cold Drawn mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 203 - 211 GPa Typical for Tool And Machining Steel
Hardness, Brinell 23.0 °C Hardness, Brinell of 285 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Tool And Machining Steel
Shear modulus 23.0 °C Shear modulus of 79 GPa Typical for Tool And Machining Steel