ASTM A681 Grade Type A2 Cold Drawn
Equivalent material: DIN 1.2363, DIN X100CrMoV5-1, DIN X100CrMoV5, AFNOR Z100CDV5, AFNOR X100CrMoV5, BS X100CrMoV5, BS BA2, AISI A2, SAE A2, JIS SKD12, EN X100CrMoV5, EN X100CrMoV51, EN 1.2363, ISO X100CrMoV5, UNS T30102
ASTM A681 Grade Type A2 Cold Drawn general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.72 - 8 g/cm³ |
Typical for Tool And Machining Steel |
ASTM A681 Grade Type A2 Cold Drawn thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Tool And Machining Steel |
Melting point |
- |
Melting point of 1370 - 1425 °C |
Typical for Tool And Machining Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 460 J/(kg·K) |
Typical for Tool And Machining Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 17 - 42 W/(m·K) |
Typical for Tool And Machining Steel |
ASTM A681 Grade Type A2 Cold Drawn chemical
Property |
Value |
Carbon |
Carbon of 0.95 - 1.05 % |
Chromium |
Chromium of 4.75 - 5.5 % |
Manganese |
Manganese of 0.4 - 1 % |
Molybdenum |
Molybdenum of 0.9 - 1.4 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.1 - 0.5 % |
Sulfur |
Sulfur of 0.03 % |
Vanadium |
Vanadium of 0.15 - 0.5 % |
ASTM A681 Grade Type A2 Cold Drawn mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 203 - 211 GPa |
Typical for Tool And Machining Steel |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 262 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Tool And Machining Steel |
Shear modulus |
23.0 °C |
Shear modulus of 79 GPa |
Typical for Tool And Machining Steel |