ASTM A668 Class L Normalized, quenched, and tempered
Equivalent material: ASTM Class L, ASTM L, UNS K24045
ASTM A668 Class L Normalized, quenched, and tempered general
Property |
Temperature |
Value |
Comment |
Density |
20.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A668 Class L Normalized, quenched, and tempered thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
20.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Nickel Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 34 - 54 W/(m·K) |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A668 Class L Normalized, quenched, and tempered electrical
Property |
Value |
Phosphorus |
Phosphorus of 0.04 % |
Sulfur |
Sulfur of 0.025 % |
ASTM A668 Class L Normalized, quenched, and tempered mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 |
20.0 °C |
Elongation A50 of 14 - 16 % |
- |
Hardness, Brinell |
20.0 °C |
Hardness, Brinell of 223 - 321 [-] |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Chromium Molybdenum Steel |
Reduction of area |
20.0 °C |
Reduction of area of 40 - 50 % |
- |
Tensile strength |
20.0 °C |
Tensile strength of 760 - 860 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 585 - 725 MPa |
- |