ASTM A668 Class E Normalized and tempered or double-normalized and tempered
Equivalent material: ASTM E, UNS K14048
ASTM A668 Class E Normalized and tempered or double-normalized and tempered general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
ASTM A668 Class E Normalized and tempered or double-normalized and tempered thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
ASTM A668 Class E Normalized and tempered or double-normalized and tempered electrical
Property |
Value |
Manganese |
Manganese of 1.35 % |
Phosphorus |
Phosphorus of 0.05 % |
Sulfur |
Sulfur of 0.025 % |
ASTM A668 Class E Normalized and tempered or double-normalized and tempered mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 22 - 25 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 174 - 217 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |
Reduction of area |
23.0 °C |
Reduction of area of 35 - 40 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 570 - 585 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 295 - 305 MPa |
- |