ASTM A600 Grade Type T6 Cold Drawn
Equivalent material: UNS T12006
ASTM A600 Grade Type T6 Cold Drawn general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.72 - 8 g/cm³ |
Typical for Tool And Machining Steel |
ASTM A600 Grade Type T6 Cold Drawn thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Tool And Machining Steel |
Melting point |
- |
Melting point of 1370 - 1425 °C |
Typical for Tool And Machining Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 460 J/(kg·K) |
Typical for Tool And Machining Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 17 - 42 W/(m·K) |
Typical for Tool And Machining Steel |
ASTM A600 Grade Type T6 Cold Drawn chemical
Property |
Value |
Carbon |
Carbon of 0.75 - 0.85 % |
Chromium |
Chromium of 4 - 4.75 % |
Cobalt |
Cobalt of 11 - 13 % |
Manganese |
Manganese of 0.2 - 0.4 % |
Molybdenum |
Molybdenum of 0.4 - 1 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.2 - 0.4 % |
Sulfur |
Sulfur of 0.03 % |
Tungsten |
Tungsten of 18.5 - 21 % |
Vanadium |
Vanadium of 1.5 - 2.1 % |
ASTM A600 Grade Type T6 Cold Drawn mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 203 - 211 GPa |
Typical for Tool And Machining Steel |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 321 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Tool And Machining Steel |
Shear modulus |
23.0 °C |
Shear modulus of 79 GPa |
Typical for Tool And Machining Steel |