ASTM A600 Grade Type T2 Annealed

Equivalent material: AISI T2, SAE T2, UNS T12002

ASTM A600 Grade Type T2 Annealed general

Property Temperature Value Comment
Density 23.0 °C Density of 7.72 - 8 g/cm³ Typical for Tool And Machining Steel

ASTM A600 Grade Type T2 Annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K Typical for Tool And Machining Steel
Melting point - Melting point of 1370 - 1425 °C Typical for Tool And Machining Steel
Specific heat capacity 23.0 °C Specific heat capacity of 420 - 460 J/(kg·K) Typical for Tool And Machining Steel
Thermal conductivity 23.0 °C Thermal conductivity of 17 - 42 W/(m·K) Typical for Tool And Machining Steel

ASTM A600 Grade Type T2 Annealed chemical

Property Value
Carbon Carbon of 0.8 - 0.9 %
Chromium Chromium of 3.75 - 4.5 %
Manganese Manganese of 0.2 - 0.4 %
Molybdenum Molybdenum of 1 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.2 - 0.4 %
Sulfur Sulfur of 0.03 %
Tungsten Tungsten of 17.5 - 19 %
Vanadium Vanadium of 1.8 - 2.4 %

ASTM A600 Grade Type T2 Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 203 - 211 GPa Typical for Tool And Machining Steel
Hardness, Brinell 23.0 °C Hardness, Brinell of 255 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Tool And Machining Steel
Shear modulus 23.0 °C Shear modulus of 79 GPa Typical for Tool And Machining Steel

Our stringent quality control measures ensure consistent and reliable steel products.

-- Our promise

Similar or equivalent steel materials

Get a quote