ASTM A600 Grade Type M41 Cold Drawn
Equivalent material: DIN 1.3246, DIN S 7-4-2-5, DIN HS7-4-2-5, AFNOR Z110WKCDV07-05-04, UNI HS7-4-2-5, SS 7-4-2-5, UNE M35, AISI M41, SAE M41, EN 1.3246, GB/T T77445, GB/T W7Mo4Cr4V2Co5, UNS T11341
ASTM A600 Grade Type M41 Cold Drawn general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.72 - 8 g/cm³ |
Typical for Tool And Machining Steel |
ASTM A600 Grade Type M41 Cold Drawn thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Tool And Machining Steel |
Melting point |
- |
Melting point of 1370 - 1425 °C |
Typical for Tool And Machining Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 460 J/(kg·K) |
Typical for Tool And Machining Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 17 - 42 W/(m·K) |
Typical for Tool And Machining Steel |
ASTM A600 Grade Type M41 Cold Drawn chemical
Property |
Value |
Carbon |
Carbon of 1.05 - 1.15 % |
Chromium |
Chromium of 3.75 - 4.5 % |
Cobalt |
Cobalt of 4.75 - 5.75 % |
Manganese |
Manganese of 0.2 - 0.6 % |
Molybdenum |
Molybdenum of 3.25 - 4.25 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.15 - 0.5 % |
Sulfur |
Sulfur of 0.03 % |
Tungsten |
Tungsten of 6.25 - 7 % |
Vanadium |
Vanadium of 1.75 - 2.25 % |
ASTM A600 Grade Type M41 Cold Drawn mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 203 - 211 GPa |
Typical for Tool And Machining Steel |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 285 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Tool And Machining Steel |
Shear modulus |
23.0 °C |
Shear modulus of 79 GPa |
Typical for Tool And Machining Steel |