ASTM A597 Grade CD-2
Equivalent material: DIN 1.2379, DIN X155CrVMo12-1, DIN X153CrMoV12, DIN X155CrMoV12-1, AFNOR Z160CDV12, AFNOR X153CrMoV12, AFNOR X160CrMoV12, BS BD2, BS X153CrMoV12, UNI X155CrVMo121KU, UNE X153CrMoV12, AISI D2, SAE D2, JIS SKD11, JIS SKD10, EN X153CrMoV12, EN X160CrMoV121, EN 1.2379, ISO X153CrMoV12, GOST Ch12MF, GB Cr12MoV, GB/T Cr12Mo1V1, GB/T T21202, ASTM D2, ASTM Type D2, UNS T30402, UNS T90402
ASTM A597 Grade CD-2 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.72 - 8 g/cm³ |
Typical for Tool And Machining Steel |
ASTM A597 Grade CD-2 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Tool And Machining Steel |
Melting point |
- |
Melting point of 1370 - 1425 °C |
Typical for Tool And Machining Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 460 J/(kg·K) |
Typical for Tool And Machining Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 17 - 42 W/(m·K) |
Typical for Tool And Machining Steel |
ASTM A597 Grade CD-2 chemical
Property |
Value |
Carbon |
Carbon of 1.4 - 1.6 % |
Chromium |
Chromium of 11 - 13 % |
Cobalt |
Cobalt of 0.7 - 1 % |
Manganese |
Manganese of 1 % |
Molybdenum |
Molybdenum of 0.7 - 1.2 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 1.5 % |
Sulfur |
Sulfur of 0.03 % |
Vanadium |
Vanadium of 0.4 - 1 % |
ASTM A597 Grade CD-2 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 203 - 211 GPa |
Typical for Tool And Machining Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Tool And Machining Steel |
Shear modulus |
23.0 °C |
Shear modulus of 79 GPa |
Typical for Tool And Machining Steel |