ASTM A579 Grade 73 Type 7, Maraging
Equivalent material: DIN 1.6358, DIN X2NiCoMo18-9-5, BS NiMark250, EN X2NiCoMo18-9-5, EN 1.6358, ASTM Grade 73
ASTM A579 Grade 73 Type 7, Maraging general
Property |
Temperature |
Value |
Comment |
Density |
20.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Molybdenum Steel |
ASTM A579 Grade 73 Type 7, Maraging thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
20.0 °C |
Coefficient of thermal expansion of 9E-6 - 1.3E-5 1/K |
Typical for Nickel Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Molybdenum Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 44 W/(m·K) |
Typical for Nickel Molybdenum Steel |
ASTM A579 Grade 73 Type 7, Maraging chemical
Property |
Value |
Aluminium |
Aluminium of 0.05 - 0.15 % |
Carbon |
Carbon of 0.03 % |
Cobalt |
Cobalt of 8.5 - 9.5 % |
Manganese |
Manganese of 0.1 % |
Molybdenum |
Molybdenum of 4.6 - 5.2 % |
Nickel |
Nickel of 18 - 19 % |
Phosphorus |
Phosphorus of 0.01 % |
Silicon |
Silicon of 0.1 % |
Sulfur |
Sulfur of 0.01 % |
Titanium |
Titanium of 0.5 - 0.8 % |
ASTM A579 Grade 73 Type 7, Maraging mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
20.0 °C |
Charpy impact energy of 20 J |
- |
Elastic modulus |
20.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Molybdenum Steel |
Elongation |
20.0 °C |
Elongation of 9 % |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Molybdenum Steel |
Reduction of area |
20.0 °C |
Reduction of area of 40 % |
- |
Tensile strength |
20.0 °C |
Tensile strength of 1930 MPa |
- |
Yield Strength Rp0.2, short transverse |
20.0 °C |
Yield Strength Rp0.2, short transverse of 1895 MPa |
- |