ASTM A494 Grade M25S

ASTM A494 Grade M25S general

Property Temperature Value Comment
Density 23.0 °C Density of 8.8 g/cm³ Typical for Nickel Steel

ASTM A494 Grade M25S thermal

Property Temperature Value Comment
Melting point - Melting point of 1316 - 1595 °C Typical for Nickel Steel
Specific heat capacity 23.0 °C Specific heat capacity of 456 J/(kg·K) Typical for Nickel Steel
Thermal conductivity 23.0 °C Thermal conductivity of 10 - 50 W/(m·K) Typical for Nickel Steel

ASTM A494 Grade M25S chemical

Property Value
Carbon Carbon of 0.25 %
Copper Copper of 27 - 33 %
Iron Iron of 3.5 %
Manganese Manganese of 1.5 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 3.5 - 4.5 %
Sulfur Sulfur of 0.02 %

ASTM A494 Grade M25S mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Steel
Hardness, Brinell 23.0 °C Hardness, Brinell of 300 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Steel
Shear modulus 23.0 °C Shear modulus of 76 GPa Typical for Nickel Steel