ASTM A487 Grade 13 Class A, Heat-Treated
ASTM A487 Grade 13 Class A, Heat-Treated general
| Property | Temperature | Value |
|---|---|---|
| Elongation A50 | 20.0 °C | Elongation A50 of 18 % |
| Reduction of area | 20.0 °C | Reduction of area of 35 % |
| Tensile strength | 20.0 °C | Tensile strength of 620 MPa |
| Yield Strength Rp0.2, short transverse | 20.0 °C | Yield Strength Rp0.2, short transverse of 415 MPa |
ASTM A487 Grade 13 Class A, Heat-Treated chemical
| Property | Value |
|---|---|
| Boron | Boron of 0.4 % |
| Carbon | Carbon of 0.3 % |
| Copper | Copper of 0.1 % |
| Manganese | Manganese of 0.8 - 1.1 % |
| Molybdenum | Molybdenum of 0.2 - 0.3 % |
| Nickel | Nickel of 0.03 % |
| Phosphorus | Phosphorus of 0.04 % |
| Silicon | Silicon of 0.6 % |
| Sulfur | Sulfur of 0.035 % |