ASTM A479 Grade S32101 Annealed

Equivalent material: DIN 1.4162, JIS LDX 2101, EN X2CrMnNiN21-5-1, EN 1.4162, UNS S32101

ASTM A479 Grade S32101 Annealed general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 g/cm³ Typical for Duplex Stainless Steel

ASTM A479 Grade S32101 Annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1E-5 1/K Typical for Duplex Stainless Steel
Max service temperature - Max service temperature of 300 °C Typical for Duplex Stainless Steel
Melting point - Melting point of 1375 - 1450 °C Typical for Duplex Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 - 502 J/(kg·K) Typical for Duplex Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 13 - 30 W/(m·K) Typical for Duplex Stainless Steel

ASTM A479 Grade S32101 Annealed chemical

Property Value
Carbon Carbon of 0.04 %
Chromium Chromium of 21 - 22 %
Manganese Manganese of 4 - 6 %
Molybdenum Molybdenum of 0.1 - 0.8 %
Nickel Nickel of 1.35 - 1.7 %
Nitrogen Nitrogen of 0.2 - 0.25 %
Phosphorus Phosphorus of 0.04 %
Silicon Silicon of 1 %
Sulfur Sulfur of 0.03 %

ASTM A479 Grade S32101 Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 GPa Typical for Duplex Stainless Steel
Elongation A50 23.0 °C Elongation A50 of 30 % -
Hardness, Brinell 23.0 °C Hardness, Brinell of 290 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Duplex Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Duplex Stainless Steel
Tensile strength 23.0 °C Tensile strength of 650 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 450 MPa -

Drive progress and development with our high-performance steel materials.