ASTM A471 Class 14 Heat-Treated
ASTM A471 Class 14 Heat-Treated general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
ASTM A471 Class 14 Heat-Treated thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Melting point | - | Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
ASTM A471 Class 14 Heat-Treated chemical
Property | Value |
---|---|
Aluminium | Aluminium of 0.015 % |
Carbon | Carbon of 0.45 % |
Chromium | Chromium of 0.5 - 1.25 % |
Manganese | Manganese of 0.6 - 1 % |
Molybdenum | Molybdenum of 0.2 % |
Nickel | Nickel of 1.65 - 3.5 % |
Phosphorus | Phosphorus of 0.01 % |
Sulfur | Sulfur of 0.015 % |
ASTM A471 Class 14 Heat-Treated mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | Charpy impact energy of 20 J | - |
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 | 23.0 °C | Elongation A50 of 18 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 255 - 302 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Reduction of area | 23.0 °C | Reduction of area of 45 % | - |
Tensile strength | 23.0 °C | Tensile strength of 860 MPa | - |
Yield strength Rp0.02 | 23.0 °C | Yield strength Rp0.02 of 725 - 860 MPa | - |