ASTM A470 Grade D Class 8 Double-Normalized and Tempered

Equivalent material: UNS K23010

ASTM A470 Grade D Class 8 Double-Normalized and Tempered general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Chromium Molybdenum Steel

ASTM A470 Grade D Class 8 Double-Normalized and Tempered thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K Typical for Chromium Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Chromium Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 448 - 502 J/(kg·K) Typical for Chromium Molybdenum Steel
Thermal conductivity 23.0 °C Thermal conductivity of 36 - 43 W/(m·K) Typical for Chromium Molybdenum Steel

ASTM A470 Grade D Class 8 Double-Normalized and Tempered chemical

Property Value
Aluminium Aluminium of 0.015 %
Carbon Carbon of 0.25 - 0.35 %
Chromium Chromium of 1.05 - 1.5 %
Manganese Manganese of 1 %
Molybdenum Molybdenum of 1 - 1.5 %
Nickel Nickel of 0.75 %
Phosphorus Phosphorus of 0.01 %
Sulfur Sulfur of 0.015 %
Vanadium Vanadium of 0.2 - 0.3 %

ASTM A470 Grade D Class 8 Double-Normalized and Tempered mechanical

Property Temperature Value Comment
Charpy impact energy 23.0 °C Charpy impact energy of 8 J -
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Chromium Molybdenum Steel
Elongation A50 23.0 °C Elongation A50 of 17 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Chromium Molybdenum Steel
Reduction of area 23.0 °C Reduction of area of 43 % -
Tensile strength 23.0 °C Tensile strength of 725 - 860 MPa -
Yield strength 23.0 °C Yield strength of 585 MPa -
Yield strength Rp0.02 23.0 °C Yield strength Rp0.02 of 585 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 620 MPa -