ASTM A439 Grade Type D-5 As-Cast or Heat-Treated
ASTM A439 Grade Type D-5 As-Cast or Heat-Treated general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 8.8 g/cm³ | Typical for Nickel Steel |
ASTM A439 Grade Type D-5 As-Cast or Heat-Treated thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | - | Melting point of 1316 - 1595 °C | Typical for Nickel Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
ASTM A439 Grade Type D-5 As-Cast or Heat-Treated chemical
Property | Value |
---|---|
Carbon | Carbon of 2.4 % |
Chromium | Chromium of 0.1 % |
Manganese | Manganese of 1 % |
Nickel | Nickel of 34 - 36 % |
Phosphorus | Phosphorus of 0.08 % |
Silicon | Silicon of 1 - 2.8 % |
ASTM A439 Grade Type D-5 As-Cast or Heat-Treated mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
Elongation A50 | 23.0 °C | Elongation A50 of 20 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 131 - 185 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
Shear modulus | 23.0 °C | Shear modulus of 76 GPa | Typical for Nickel Steel |
Tensile strength | 23.0 °C | Tensile strength of 380 MPa | - |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 210 MPa | - |