ASTM A439 Grade Type D-2 As-Cast or Heat-Treated
ASTM A439 Grade Type D-2 As-Cast or Heat-Treated general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 8.8 g/cm³ | Typical for Nickel Steel |
ASTM A439 Grade Type D-2 As-Cast or Heat-Treated thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Melting point | - | Melting point of 1316 - 1595 °C | Typical for Nickel Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
ASTM A439 Grade Type D-2 As-Cast or Heat-Treated chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 3 % |
| Chromium | Chromium of 1.75 - 2.75 % |
| Manganese | Manganese of 0.7 - 1.25 % |
| Nickel | Nickel of 18 - 22 % |
| Phosphorus | Phosphorus of 0.08 % |
| Silicon | Silicon of 1.5 - 3 % |
ASTM A439 Grade Type D-2 As-Cast or Heat-Treated mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
| Elongation A50 | 23.0 °C | Elongation A50 of 8 % | - |
| Hardness, Brinell | 23.0 °C | Hardness, Brinell of 139 - 202 [-] | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
| Shear modulus | 23.0 °C | Shear modulus of 76 GPa | Typical for Nickel Steel |
| Tensile strength | 23.0 °C | Tensile strength of 400 MPa | - |
| Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 210 MPa | - |