ASTM A409 Grade N08367 Heat-Treated
ASTM A409 Grade N08367 Heat-Treated general
| Property | Temperature | Value |
|---|---|---|
| Tensile strength | 23.0 °C | Tensile strength of 655 - 690 MPa |
| Yield strength | 23.0 °C | Yield strength of 310 MPa |
ASTM A409 Grade N08367 Heat-Treated chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.03 % |
| Chromium | Chromium of 20 - 22 % |
| Manganese | Manganese of 2 % |
| Molybdenum | Molybdenum of 6 - 7 % |
| Nickel | Nickel of 23.5 - 25.5 % |
| Phosphorus | Phosphorus of 0.04 % |
| Silicon | Silicon of 1 % |
| Sulfur | Sulfur of 0.03 % |
We offer top-notch steel without compromising on quality or affordability.
-- Our promise

Get a quote