ASTM A403 Grade N08926 Heat-Treated
ASTM A403 Grade N08926 Heat-Treated general
| Property | Temperature | Value |
|---|---|---|
| Elongation A50 | 23.0 °C | Elongation A50 of 20 - 28 % |
| Tensile strength | 23.0 °C | Tensile strength of 650 MPa |
| Yield strength | 23.0 °C | Yield strength of 295 MPa |
ASTM A403 Grade N08926 Heat-Treated chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.02 % |
| Chromium | Chromium of 19 - 21 % |
| Manganese | Manganese of 2 % |
| Molybdenum | Molybdenum of 6 - 7 % |
| Nickel | Nickel of 24 - 26 % |
| Nitrogen | Nitrogen of 0.15 - 0.25 % |
| Phosphorus | Phosphorus of 0.03 % |
| Silicon | Silicon of 0.5 % |
| Sulfur | Sulfur of 0.01 % |