ASTM A372 Grade K Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and Temper

Equivalent material: ASTM Grade K

ASTM A372 Grade K Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and Temper general

Property Temperature Value Comment
Density 20.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Nickel Chromium Molybdenum Steel

ASTM A372 Grade K Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and Temper thermal

Property Temperature Value Comment
Coefficient of thermal expansion 20.0 °C Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K Typical for Nickel Chromium Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Nickel Chromium Molybdenum Steel
Thermal conductivity 20.0 °C Thermal conductivity of 34 - 54 W/(m·K) Typical for Nickel Chromium Molybdenum Steel

ASTM A372 Grade K Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and Temper chemical

Property Value
Carbon Carbon of 0.18 %
Chromium Chromium of 1 - 1.8 %
Manganese Manganese of 0.1 - 0.4 %
Molybdenum Molybdenum of 0.2 - 0.6 %
Nickel Nickel of 2 - 3.3 %
Phosphorus Phosphorus of 0.02 %
Silicon Silicon of 0.15 - 0.35 %
Sulfur Sulfur of 0.01 %

ASTM A372 Grade K Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and Temper mechanical

Property Temperature Value Comment
Elastic modulus 20.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Chromium Molybdenum Steel
Elongation A50 20.0 °C Elongation A50 of 20 % -
Hardness, Brinell 20.0 °C Hardness, Brinell of 207 [-] -
Poisson's ratio 20.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Chromium Molybdenum Steel
Tensile strength 20.0 °C Tensile strength of 690 - 860 MPa -
Yield Strength Rp0.2, short transverse 20.0 °C Yield Strength Rp0.2, short transverse of 550 MPa -