ASTM A352 Grade LC9 Normalized and Tempered or Liquid Quenched and Tempered

Equivalent material: UNS J31300, 9Ni

ASTM A352 Grade LC9 Normalized and Tempered or Liquid Quenched and Tempered general

Property Temperature Value Comment
Density 23.0 °C Density of 8.8 g/cm³ Typical for Nickel Steel

ASTM A352 Grade LC9 Normalized and Tempered or Liquid Quenched and Tempered thermal

Property Temperature Value Comment
Melting point - Melting point of 1316 - 1595 °C Typical for Nickel Steel
Specific heat capacity 23.0 °C Specific heat capacity of 456 J/(kg·K) Typical for Nickel Steel
Thermal conductivity 23.0 °C Thermal conductivity of 10 - 50 W/(m·K) Typical for Nickel Steel

ASTM A352 Grade LC9 Normalized and Tempered or Liquid Quenched and Tempered chemical

Property Value
Carbon Carbon of 0.13 %
Chromium Chromium of 0.5 %
Copper Copper of 0.3 %
Manganese Manganese of 0.9 %
Molybdenum Molybdenum of 0.2 %
Nickel Nickel of 8.5 - 10 %
Phosphorus Phosphorus of 0.04 %
Silicon Silicon of 0.45 %
Sulfur Sulfur of 0.045 %
Vanadium Vanadium of 0.03 %

ASTM A352 Grade LC9 Normalized and Tempered or Liquid Quenched and Tempered mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Steel
Elongation A50 23.0 °C Elongation A50 of 20 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Steel
Reduction of area 23.0 °C Reduction of area of 30 % -
Shear modulus 23.0 °C Shear modulus of 76 GPa Typical for Nickel Steel
Tensile strength 23.0 °C Tensile strength of 585 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 515 MPa -