ASTM A352 Grade LC4 Normalized and Tempered or Liquid Quenched and Tempered
Equivalent material: UNS J41500, 4.5Ni
ASTM A352 Grade LC4 Normalized and Tempered or Liquid Quenched and Tempered general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 8.8 g/cm³ | Typical for Nickel Steel |
ASTM A352 Grade LC4 Normalized and Tempered or Liquid Quenched and Tempered thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Melting point | - | Melting point of 1316 - 1595 °C | Typical for Nickel Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
ASTM A352 Grade LC4 Normalized and Tempered or Liquid Quenched and Tempered chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.15 % |
| Manganese | Manganese of 0.5 - 0.8 % |
| Nickel | Nickel of 4 - 5 % |
| Phosphorus | Phosphorus of 0.04 % |
| Silicon | Silicon of 0.6 % |
| Sulfur | Sulfur of 0.045 % |
ASTM A352 Grade LC4 Normalized and Tempered or Liquid Quenched and Tempered mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Charpy impact energy | 23.0 °C | Charpy impact energy of 20 J | - |
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
| Elongation A50 | 23.0 °C | Elongation A50 of 24 % | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
| Reduction of area | 23.0 °C | Reduction of area of 35 % | - |
| Shear modulus | 23.0 °C | Shear modulus of 76 GPa | Typical for Nickel Steel |
| Tensile strength | 23.0 °C | Tensile strength of 485 - 655 MPa | - |
| Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 275 MPa | - |