ASTM A333 Grade 9 Heat-Treated general
| Property | Temperature | Value |
|---|---|---|
| Charpy impact energy | 23.0 °C | Charpy impact energy of 18 J |
| Elongation A50 | 23.0 °C | Elongation A50 of 28 % |
| Tensile strength | 23.0 °C | Tensile strength of 435 MPa |
| Yield strength | 23.0 °C | Yield strength of 315 MPa |
ASTM A333 Grade 9 Heat-Treated chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.2 % |
| Copper | Copper of 0.75 - 1.25 % |
| Manganese | Manganese of 0.4 - 1.06 % |
| Nickel | Nickel of 1.6 - 2.24 % |
| Phosphorus | Phosphorus of 0.03 % |
| Sulfur | Sulfur of 0.025 % |