ASTM A333 Grade 4 Heat-Treated
ASTM A333 Grade 4 Heat-Treated general
| Property | Temperature | Value |
|---|---|---|
| Charpy impact energy | 23.0 °C | Charpy impact energy of 18 J |
| Elongation A50 | 23.0 °C | Elongation A50 of 16.5 - 30 % |
| Tensile strength | 23.0 °C | Tensile strength of 415 MPa |
| Yield strength | 23.0 °C | Yield strength of 240 MPa |
ASTM A333 Grade 4 Heat-Treated chemical
| Property | Value |
|---|---|
| Aluminium | Aluminium of 0.04 - 0.3 % |
| Carbon | Carbon of 0.12 % |
| Chromium | Chromium of 0.44 - 1.01 % |
| Copper | Copper of 0.4 - 0.75 % |
| Manganese | Manganese of 0.5 - 1.05 % |
| Nickel | Nickel of 0.47 - 0.98 % |
| Phosphorus | Phosphorus of 0.03 % |
| Silicon | Silicon of 0.08 - 0.37 % |
| Sulfur | Sulfur of 0.025 % |