ASTM A333 Grade 3 Heat-Treated
ASTM A333 Grade 3 Heat-Treated general
| Property | Temperature | Value |
|---|---|---|
| Charpy impact energy | 23.0 °C | Charpy impact energy of 18 J |
| Elongation A50 | 23.0 °C | Elongation A50 of 20 - 30 % |
| Tensile strength | 23.0 °C | Tensile strength of 450 MPa |
| Yield strength | 23.0 °C | Yield strength of 240 MPa |
ASTM A333 Grade 3 Heat-Treated chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.19 % |
| Manganese | Manganese of 0.31 - 0.64 % |
| Nickel | Nickel of 3.18 - 3.82 % |
| Phosphorus | Phosphorus of 0.03 % |
| Silicon | Silicon of 0.18 - 0.37 % |
| Sulfur | Sulfur of 0.025 % |
Tailor-made to fit your specific requirements, our steel solutions deliver optimal results.
-- Our promise

Get a quote