ASTM A333 Grade 1 Heat-Treated

ASTM A333 Grade 1 Heat-Treated general

Property Temperature Value
Charpy impact energy 23.0 °C Charpy impact energy of 18 J
Elongation A50 23.0 °C Elongation A50 of 25 - 35 %
Tensile strength 23.0 °C Tensile strength of 380 MPa
Yield strength 23.0 °C Yield strength of 205 MPa

ASTM A333 Grade 1 Heat-Treated chemical

Property Value
Carbon Carbon of 0.3 %
Manganese Manganese of 0.4 - 1.06 %
Phosphorus Phosphorus of 0.03 %
Sulfur Sulfur of 0.025 %