ASTM A311 Grade 1137 Normal Draft Cold Drawn and Stress Relief Annealed

Equivalent material: DIN 1.0764, DIN 36SMn14, AFNOR 36SMn14, BS 36SMn14, BS 216M36, AISI 1137, SAE 1137, JIS SUM41, EN 36SMn14, EN 1.0764, ISO 36SMn14, ASTM 1137, UNS G11370, DIN 1.0765, DIN 35MF6Pb14, AFNOR 35MF6Pb14, BS 35MF6Pb14, AISI 11L37, SAE 11L37, EN 36SMnPb14, EN 1.0765, ISO 35MF6Pb14, GOST AS35G2

ASTM A311 Grade 1137 Normal Draft Cold Drawn and Stress Relief Annealed general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Manganese Steel

ASTM A311 Grade 1137 Normal Draft Cold Drawn and Stress Relief Annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.33E-5 1/K Typical for Manganese Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Manganese Steel
Specific heat capacity 23.0 °C Specific heat capacity of 510 - 553 J/(kg·K) Typical for Manganese Steel
Thermal conductivity 23.0 °C Thermal conductivity of 14 - 16 W/(m·K) Typical for Manganese Steel

ASTM A311 Grade 1137 Normal Draft Cold Drawn and Stress Relief Annealed chemical

Property Value
Carbon Carbon of 0.32 - 0.39 %
Manganese Manganese of 1.35 - 1.65 %
Phosphorus Phosphorus of 0.04 %
Sulfur Sulfur of 0.08 - 0.13 %

ASTM A311 Grade 1137 Normal Draft Cold Drawn and Stress Relief Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Manganese Steel
Elongation A50 23.0 °C Elongation A50 of 10 - 11 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Manganese Steel
Reduction of area 23.0 °C Reduction of area of 30 - 35 % -
Tensile strength 23.0 °C Tensile strength of 550 - 655 MPa -
Yield strength 23.0 °C Yield strength of 520 - 620 MPa -