ASTM A240 Grade S35045 Heat-Treated
Equivalent material: UNS S35045
ASTM A240 Grade S35045 Heat-Treated general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 8.8 g/cm³ |
Typical for Nickel Steel |
ASTM A240 Grade S35045 Heat-Treated thermal
| Property |
Temperature |
Value |
Comment |
| Melting point |
- |
Melting point of 1316 - 1595 °C |
Typical for Nickel Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 456 J/(kg·K) |
Typical for Nickel Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 10 - 50 W/(m·K) |
Typical for Nickel Steel |
ASTM A240 Grade S35045 Heat-Treated chemical
| Property |
Value |
| Carbon |
Carbon of 0.06 - 0.1 % |
| Chromium |
Chromium of 25 - 29 % |
| Copper |
Copper of 0.75 % |
| Manganese |
Manganese of 1.5 % |
| Nickel |
Nickel of 32 - 37 % |
| Phosphorus |
Phosphorus of 0.05 % |
| Silicon |
Silicon of 1 % |
| Sulfur |
Sulfur of 0.015 % |
ASTM A240 Grade S35045 Heat-Treated mechanical
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Steel |
| Elongation A50 |
23.0 °C |
Elongation A50 of 35 % |
- |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Steel |
| Shear modulus |
23.0 °C |
Shear modulus of 76 GPa |
Typical for Nickel Steel |
| Tensile strength |
23.0 °C |
Tensile strength of 485 MPa |
- |
| Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 170 MPa |
- |