ASTM A213 Grade T17
Equivalent material: UNS K12047
ASTM A213 Grade T17 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Vanadium Steel |
ASTM A213 Grade T17 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.2E-5 1/K |
Typical for Chromium Vanadium Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Vanadium Steel |
ASTM A213 Grade T17 chemical
Property |
Value |
Carbon |
Carbon of 0.15 - 0.25 % |
Chromium |
Chromium of 0.8 - 1.25 % |
Manganese |
Manganese of 0.3 - 0.61 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.025 % |
Vanadium |
Vanadium of 0.15 % |
ASTM A213 Grade T17 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Vanadium Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Vanadium Steel |