ASTM A213 Grade 800H Heat-Treated
ASTM A213 Grade 800H Heat-Treated general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
ASTM A213 Grade 800H Heat-Treated thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Melting point | - | Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
ASTM A213 Grade 800H Heat-Treated chemical
Property | Value |
---|---|
Carbon | Carbon of 0.05 - 0.1 % |
Chromium | Chromium of 19 - 23 % |
Manganese | Manganese of 1.5 % |
Nickel | Nickel of 30 - 35 % |
Phosphorus | Phosphorus of 0.05 % |
Silicon | Silicon of 1 % |
Sulfur | Sulfur of 0.015 % |
ASTM A213 Grade 800H Heat-Treated electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | Electrical resistivity of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
ASTM A213 Grade 800H Heat-Treated mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 195 GPa | Typical for Austenitic Stainless Steel |
Elongation A50 | 23.0 °C | Elongation A50 of 30 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 192 [-] | - |
Hardness, Rockwell B | 23.0 °C | Hardness, Rockwell B of 90 [-] | - |
Hardness, Vickers | 23.0 °C | Hardness, Vickers of 200 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 23.0 °C | Tensile strength of 450 MPa | - |
Yield strength | 23.0 °C | Yield strength of 170 MPa | - |