ASTM A209 Grade T1B Heat-Treated
ASTM A209 Grade T1B Heat-Treated general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
ASTM A209 Grade T1B Heat-Treated thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.29E-5 1/K | Typical for Molybdenum Steel |
| Melting point | - | Melting point of 1382 - 1529 °C | Typical for Molybdenum Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Molybdenum Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |
ASTM A209 Grade T1B Heat-Treated chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.14 % |
| Manganese | Manganese of 0.3 - 0.8 % |
| Molybdenum | Molybdenum of 0.44 - 0.65 % |
| Phosphorus | Phosphorus of 0.03 % |
| Silicon | Silicon of 0.1 - 0.5 % |
| Sulfur | Sulfur of 0.025 % |
ASTM A209 Grade T1B Heat-Treated mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Molybdenum Steel |
| Elongation A50 | 23.0 °C | Elongation A50 of 30 % | - |
| Hardness, Brinell | 23.0 °C | Hardness, Brinell of 137 [-] | - |
| Hardness, Rockwell B | 23.0 °C | Hardness, Rockwell B of 77 [-] | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Molybdenum Steel |
| Tensile strength | 23.0 °C | Tensile strength of 365 MPa | - |
| Yield strength | 23.0 °C | Yield strength of 195 MPa | - |