ASME SA479 Grade 316
Equivalent material: DIN 1.4401, DIN 316S42, DIN 316S33, DIN X5CrNiMo17-12-2, DIN X 5 CrNiMo 18 10, AFNOR Z7CND17-11-02, BS 316S16, UNI X5CrNiMo1712, SS 2347, UNE F.3543, AISI 316, JIS SUS316, JIS SUS316TKA, JIS SUS316TF, JIS SUS316FB, JIS SUSF316, JIS SUS316TKC, JIS SUS316TP, JIS SUS316TB, JIS SUS316TBS, JIS SUS316TPY, JIS SUS316TPD, JIS SUS316HTP, JIS SUS316HTB, JIS SUS316HTF, JIS SUS316F, EN X5CrNiMo17-12-2, EN 1.4401, ISO A4, GOST 0Cr17Ni12Mo2, GB 08Ch27N13M2, ASTM 316, UNS S31600, IS X04Cr17Ni12Mo2, DIN 1.4436, DIN X5CrNiMo17-13-3, DIN X3CrNiMo17-13-3, AFNOR Z7CND18-12-03, BS 316S13, UNI X8CrNiMo1713, SS 2343, JIS SCS14, EN X3CrNiMo17-13-3, EN 1.4436, ISO A5, DIN 1.4984, AFNOR 9165-041, AFNOR 9165 25, AFNOR Z 10 CNW 17, EN 1.4984, ASTM F316, ASTM S31600, ASTM TP316, ASTM B8M, ASTM Grade HE35, ASTM Grade 8M, ASTM FP316, ASTM MT316, ASTM Grade 8MA, ASTM Grade B8M, ASTM Grade B8MA, ASTM Grade B8M2, ASTM Grade B8M3
ASME SA479 Grade 316 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
ASME SA479 Grade 316 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
ASME SA479 Grade 316 chemical
Property |
Value |
Carbon |
Carbon of 0.035 % |
Chromium |
Chromium of 16 - 20 % |
Manganese |
Manganese of 2 % |
Molybdenum |
Molybdenum of 2 - 3 % |
Nickel |
Nickel of 10 - 15 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.75 % |
Sulfur |
Sulfur of 0.03 % |
ASME SA479 Grade 316 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
ASME SA479 Grade 316 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Experience a new standard of excellence as we redefine the benchmark in the steel industry, delivering unmatched quality and service.
-- Our promise
Similar or equivalent steel materials