AS 3678 Grade 250 Hot Rolled
AS 3678 Grade 250 Hot Rolled general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
AS 3678 Grade 250 Hot Rolled thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.15E-5 1/K | - |
Max service temperature | - | Max service temperature of 500 °C | Typical for Carbon Steel |
Melting point | - | Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
AS 3678 Grade 250 Hot Rolled chemical
Property | Value |
---|---|
Carbon | Carbon of 0.22 % |
Manganese | Manganese of 1.7 % |
Phosphorus | Phosphorus of 0.04 % |
Silicon | Silicon of 0.55 % |
Sulfur | Sulfur of 0.03 % |
AS 3678 Grade 250 Hot Rolled magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | Curie temperature of 770 °C | Typical for Low Carbon Steel |
AS 3678 Grade 250 Hot Rolled electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
AS 3678 Grade 250 Hot Rolled mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel |
Elongation | 23.0 °C | Elongation of 22 % | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel |
Shear modulus | 23.0 °C | Shear modulus of 82 GPa | Typical for Low Carbon Steel |
Tensile strength | 23.0 °C | Tensile strength of 410 MPa | - |
Yield strength | 23.0 °C | Yield strength of 280 MPa | - |