AISI 304N 1/8-Hard
Equivalent material: DIN 1.4315, BS 304S65, SAE 304N, JIS SUS304N1, JIS SCS13A, JIS SUSF304N, EN X5CrNiN19-9, EN 1.4315, ASTM TP304N, UNS S30451, ASTM 304N, ASTM S30451, JIS SUSF304N, ASTM F304N, ASTM Grade 8N, ASTM 304N, ASTM FP304N, ASTM Grade B8N, ASTM Grade B8NA, ASTM Grade 8NA
AISI 304N 1/8-Hard general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
AISI 304N 1/8-Hard thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1425 - 1530 °C |
Typical for Ferritic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 500 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 15 W/(m·K) |
- |
AISI 304N 1/8-Hard chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.08 % |
Chromium |
Chromium of 18 - 20 % |
Iron |
Iron of 65.7 - 73.9 % |
Manganese |
Manganese of 0 - 2 % |
Nickel |
Nickel of 8 - 11 % |
Nitrogen |
Nitrogen of 0.1 - 0.22 % |
Phosphorus |
Phosphorus of 0 - 0.05 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 304N 1/8-Hard electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 6E-7 - 7.5E-7 Ω·m |
Typical for Ferritic Stainless Steel |
AISI 304N 1/8-Hard mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 GPa |
- |
Elongation |
23.0 °C |
Elongation of 43 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Ferritic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Ferritic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 790 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 440 MPa |
- |
Our state-of-the-art facilities ensure precision manufacturing and impeccable finishes.
-- Our promise
Similar or equivalent steel materials