AISI 204 Quarter-Hard
Equivalent material: AISI S20400, SAE S20400, SAE 204, ASTM S20400, UNS S20400
AISI 204 Quarter-Hard general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.7 g/cm³ |
AISI 204 Quarter-Hard thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 460 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
AISI 204 Quarter-Hard chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.03 % |
Chromium |
Chromium of 15 - 17 % |
Iron |
Iron of 69.6 - 76.4 % |
Manganese |
Manganese of 7 - 9 % |
Nickel |
Nickel of 1.5 - 3 % |
Nitrogen |
Nitrogen of 0.15 - 0.3 % |
Phosphorus |
Phosphorus of 0 - 0.04 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 204 Quarter-Hard electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
AISI 204 Quarter-Hard mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
- |
Elongation |
23.0 °C |
Elongation of 23 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 1110 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 1100 MPa |
- |
From concept to completion, we deliver excellence in every aspect of the steel supply chain.
-- Our promise
Similar or equivalent steel materials