AISI 201 Annealed
Equivalent material: DIN 1.4372, DIN X12CrMnNiN17-7-5, SAE 201, JIS SUS201, EN X12CrMnNiN17-7-5, EN 1.4372, ISO X12CrMnNiN17-7-5, ISO 4372-201-00-I, ISO AP29O, ISO 13, ASTM TP201, ASTM 201-1, ASTM 201-2, UNS S20100, ASTM 201
AISI 201 Annealed general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.7 g/cm³ |
AISI 201 Annealed thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 500 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 15 W/(m·K) |
- |
AISI 201 Annealed chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.15 % |
Chromium |
Chromium of 16 - 18 % |
Iron |
Iron of 67.5 - 75 % |
Manganese |
Manganese of 5.5 - 7.5 % |
Nickel |
Nickel of 3.5 - 5.5 % |
Nitrogen |
Nitrogen of 0 - 0.25 % |
Phosphorus |
Phosphorus of 0 - 0.06 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 201 Annealed electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
AISI 201 Annealed mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 GPa |
- |
Elongation |
23.0 °C |
Elongation of 46 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 660 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 310 MPa |
- |
From sourcing to delivery, we are your trusted partner, offering comprehensive steel solutions tailored to your requirements.
-- Our promise
Similar or equivalent steel materials