AISI 1020 Cold Rolled
AISI 1020 Cold Rolled general
| Property | Temperature | Value |
|---|---|---|
| Density | 23.0 °C | Density of 7.8 g/cm³ |
AISI 1020 Cold Rolled thermal
| Property | Temperature | Value |
|---|---|---|
| Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.19E-5 1/K |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 486 J/(kg·K) |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 51.9 W/(m·K) |
AISI 1020 Cold Rolled chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.18 - 0.23 % |
| Copper | Copper of 0.2 % |
| Iron | Balance |
| Manganese | Manganese of 0.3 - 0.6 % |
| Phosphorus | Phosphorus of 0.04 % |
| Sulfur | Sulfur of 0.05 % |
AISI 1020 Cold Rolled electrical
| Property | Temperature | Value |
|---|---|---|
| Electrical resistivity | 23.0 °C | Electrical resistivity of 1.59E-7 Ω·m |
AISI 1020 Cold Rolled mechanical
| Property | Temperature | Value |
|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 GPa |
| Elongation | 23.0 °C | Elongation of 26 % |
| Tensile strength | 23.0 °C | Tensile strength of 355 - 500 MPa |
| Yield strength | 23.0 °C | Yield strength of 355 - 490 MPa |